NEOFLON Coating Powder is a high performance material made from fluoropolymer resin.
Two kinds of NEOFLON Coating Powders, NEOFLON FEP, and PFA Coating Powder, are available.
NEOFLON FEP Coating Powder is a fine powder made of tetrafluoroethylene and hexafluoropropylene copolymer and NEOFLON PFA Coating Powder is a fine powder made of tetrafluoroethylene and perfluoroalkylvinylether copolymer.
NEOFLON FEP and PFA Coating Powder are low in melt viscosity and excellent in melt fluidity which can give a coating free of pinholes. NEOFLON FEP and PFA are ideal for use as corrosion resistant linings because of their excellent thermal and chemical resistance properties.
总体
材料状态 • 已商用:当前有效
供货地区 • 北美洲
• Good Corrosion Resistance • 高 ESCR(抗应力裂纹) • 良好的流动性
性能特点 • High Purity • 抗燃 • 耐化学性良好
• 低粘度 • 良好的电气性能 • 耐气候影响性能良好
用途 • 衬里 • 涂敷应用
外观 • 白色
形式 • 粉状
加工方法 • 滚塑成型 • 涂层
物理性能 额定值单位制 测试方法
比重 2.12 到 2.17g/cm³ ASTM D792
表观密度 0.75 到 1.05g/cm³ JIS K6891
熔流率 (372°C/5.0 kg) 5.0 到 7.0g/10 min ASTM D3307
颗粒大小 2 150 到 250µm
机械性能 额定值单位制 测试方法
抗张强度 19.6 到 31.4MPa JIS K6888
伸长率 (断裂) 250 到 350% JIS K6888
摩擦系数 (与自身 - 静态) 0.050 到 0.080 Internal Method
抗泰伯磨耗 (CS-17 转轮) 5.00 到 15.0mg
硬度 额定值单位制 测试方法
硬度计硬度 (邵氏 D) 60 ASTM D2240
热性能 额定值单位制 测试方法
熔融温度 303 到 313°C ASTM D3307
补充信息 额定值单位制
Adhesion Strength - Peel Test 3 4.0 到 6.0kN/m
Contact Angle 4
Hexadecane 65.0°